Steel 55# joint bars bonded with epoxy to the rail web - full-section mechanical joint
12.9S high-strength bolts, insulating end post, bushings and washers
Dry insulation resistance over 10 MΩ, wet over 1000 Ω to TB/T 2975
Longitudinal shear load 2700/3000/3300 kN for 50/60/75 kg/m rail
Factory hot-bonded or field cold-cured, for CWR and track circuit boundaries
50/60/75 kg/m, 60E1 and drawings to EN 16843 / AREMA
Trial production to your rail section and drilling pattern
Two rails meet at a joint that has to do two contradictory things. Mechanically it must behave like continuous rail: carry the bending moment, hold gauge and let a train pass at line speed without a dip. Electrically it must behave like a gap, so the signal current in one track circuit cannot leak into the next. A glued insulated rail joint solves both by bonding a pair of steel joint bars to the rail web with a structural epoxy, then separating the two rail ends with an insulating end post and isolating every bolt from the bars with bushes and washers.
The result is a full-section assembly that can be welded into a continuously welded rail (CWR) string. That is the reason it exists: CWR leaves no room for a conventional bolted joint with an expansion gap, but a signalled line still needs electrical boundaries at signals, crossovers and turnout entries. Railway engineers sometimes describe the insulated joint as the central nervous system of the track - when a wheelset shunts the two rails inside a section, the receiver sees that section as occupied and the signalling system knows where the train is.
There are two ways to build an insulated joint, and buyers often use the names interchangeably. This page covers the bonded steel route: a rolled steel fishplate, machined to match the rail web profile, glued to the rail with epoxy and clamped by high-strength bolts. The other route is a one-piece composite bar made from glass-fibre-reinforced polymer, which is a solid non-conductive component with no separate bushes, washers or end post.
They are not substitutes. The bonded steel joint carries higher longitudinal load and is the standard choice for high-speed and heavy-haul CWR where the joint has to resist temperature forces in the rail. The composite bar is lighter and, as a one-piece moulding, has no steel body to corrode; it suits metro turnouts, crane runways and locations where maintenance access is poor. For the composite version, see our composite integral insulated fishplate page. If you send us the rail section, the axle load and the signalling arrangement, we will tell you which one fits before quoting.

A glued insulated joint is a kit, not a single plate. Eight parts have to arrive together:
l Two steel joint bars (fishplates), 55# steel or better, machined with the 1:3 or 1:4 taper that matches the rail web
l An insulating slot plate / insulation layer between bar and rail web
l An insulating end post fitted between the two rail ends
l Insulating bushes in every bolt hole
l High-strength bolts, 12.9S class, with flat washers and nuts
l Optional channel steel plate for additional stiffness
l Structural epoxy adhesive, factory hot-cure or field ambient-cure grade
l Rail ends, cut square and chamfered 0.8-1.5 mm at 45°
The parts list is short, but the interfaces are where failures start. A plain steel washer in place of an insulated one will short the track circuit directly. A bolt driven through a hole without its bush does the same. Water that gets into the bolt hole corrodes the steel, and the rust path gradually pulls the insulation resistance down - which is why sealing and drainage around the bolts matter as much as the adhesive.
The figures below are the industry specification values for a bonded insulated rail joint to TB/T 2975-2018 and the published product data for 50/60/75 kg/m and 60E1 sections. They are standard and catalogue values, not ATK test results for a specific batch. Confirm which inspection documents are available for your order when we quote.
Parameter | Typical value | Basis |
Applicable rail sections | 50 / 60 / 75 kg/m; 60E1 (UIC60); also 115RE / 136RE by drawing | TB/T 2975, supplier catalogues |
Joint bar material | 55# steel or higher, heat treated | TB/T 2975-2018 |
Bolt class | 12.9S high-strength, one-time tightening | TB/T 2975, industry practice |
Dry insulation resistance, joint | >10 MΩ | TB/T 2975-2018 |
Dry insulation resistance, joint bar | >20 MΩ | TB/T 2975-2018 |
Wet insulation resistance | >1000 Ω | TB/T 2975-2018 |
Longitudinal shear load | 2700 / 3000 / 3300 kN for 50 / 60 / 75 kg/m rail | TB/T 2975-2018 |
Relative displacement after shear test | ≤0.5 mm after unloading | TB/T 2975-2018 |
Fatigue | 2 million cycles at 180 kN, 4–5 Hz, no damage or permanent set | Project specification, TB/T 2975 |
Bolt torque | ≥1100 N·m (final tightening) | Project specification |
Bar straightness | ≤0.3 mm over 1 m (≤200 km/h); ≤0.2 mm (>200 km/h) | TB/T 2975-2018 |
Length tolerance, factory joint | ±3.0 mm for ≤12.5 m | TB/T 2975-2018 |
Adhesive | Ambient-cure or low-temperature epoxy, non-hazardous for transport | Supplier product data |
Test method, insulation | 500 V DC megohmmeter, read after 1 min | TB/T 2975, EN 16843 |
One number deserves a note. The dry value above is the acceptance threshold in the standard, not a measured ATK batch value. Published batch data from a supplier catalogue report insulation resistance above 500 MΩ in dry conditions, well above the 20 MΩ required of the joint bar. A joint that only just clears 10 MΩ on the bench has no margin left for a wet winter.
Three standard families come up in enquiries, and they are not interchangeable.
Standard | Scope | What it asks for |
TB/T 2975-2018 (China) | Glued insulated rail joints | Dry >10 MΩ, wet >1000 Ω; shear 2700/3000/3300 kN; fatigue; dimensional and installation rules |
EN 16843:2024 (Europe) | Mechanical requirements for joints in running rails, ≥46 kg/m flat-bottom rail | Tensile strength Ft,min = EAαΔT1γs (E = 210 GPa, α = 1.2×10⁻⁵ K⁻¹); 3 million repeated-bending cycles at 3–10 Hz; dry ≥10 MΩ before test, ≥150 kΩ after; wet ≥200 kΩ |
AREMA / customer specification (North America) | Bonded and encapsulated insulated joints | Factory-assembled joints to customer drawing, 4- or 6-hole bars, A-490 bolts, polyurethane or epoxy encapsulation |
The resistance numbers look inconsistent until you check the test conditions. TB/T 2975 measures a dry specimen resting on an insulating support and separately defines a wet test; EN 16843 measures before and after mechanical testing with a 500 V megohmmeter. A 1000 Ω wet reading in one system and a 200 kΩ wet reading in the other are different tests, not a better product. We quote to the standard named in the enquiry and state the test method in the quotation.
The main application is a track circuit boundary on CWR: at station entry and exit signals, at block joints, and anywhere a signalled line has to be divided into detection sections. The joint is welded into the long rail string, so it sees the full longitudinal temperature force of the rail as well as the wheel load - that is why shear capacity and fatigue life dominate the specification.

Turnouts are the second big group. Insulated joints sit at turnout entries, in crossover tracks and on depot throats where the point machine and the detection circuit have to agree. Metro and urban rail use them on slab track, where there is almost no give under the joint and the assembly takes the full impact. Heavy-haul freight and high-speed lines use the factory hot-bonded version because the service conditions are less forgiving.
They also appear at level crossings, bridge ends, traction return cut points and the boundary between electrified and non-electrified sections. Where a line has no track circuit - a yard track, an industrial siding, a crane runway - a plain or frozen joint is usually the more economical choice. Tell us the signalling arrangement in the first message; it changes which joint we recommend.
Both routes produce the same type of joint, but the logistics are different.

Factory hot-bonded joints are assembled under controlled temperature and humidity. The bars are sandblasted, the rail web is ground to bright metal, the epoxy is cured in stages, and the completed assembly is measured for straightness, length and resistance before it leaves the works. Published process descriptions quote a first heating stage at 235-245 °C for 30-35 minutes and a longer second stage, with bolt torque brought up in steps. Treat those numbers as a plant-process reference: the cure cycle and final torque follow the adhesive data sheet and the project specification. The finished assembly is delivered as a measured length of rail that can be welded straight into the CWR string. Strength and insulation are the most consistent, and this is the route for high-speed and heavy-haul work.
Field ambient-cured joints are bonded on site with a room-temperature epoxy and a clamping fixture. They are cheaper and easier to transport, and they are the usual choice for interval joints and emergency replacement. The trade-off is process control: the rail web must be dry, the ambient temperature above about 0 °C and relative humidity below roughly 60 %, and the cure window can run to 48 hours. A joint bonded in the rain with a damp rail web will pass a resistance test on the day and fail a year later.
Fitting a glued joint is closer to a controlled assembly than a track task. Before the joint goes in, the 20 m of track on either side should be brought up to the line maintenance acceptance standard. The two joints on the left and right rail should be placed opposite each other, with the insulating end post at least 100 mm clear of the sleeper edge. The rail ends are cut square, chamfered 0.8-1.5 mm at 45°, then ground or sandblasted free of rust, oil, mill marks and moisture.

Bolts, nuts and washers are used as a matched set by batch number and are never forced through a hole. Torque is applied in stages and recorded; the final value is at least 1100 N·m on high-strength assemblies. Before the assembly goes into track, measure its insulation resistance with it resting on a dry insulating support - the pre-installation reading should exceed 1000 Ω. On site, a wet test can be made by pouring about 2 L of water at the end post and reading with a multimeter after one to two minutes.
Do not strike the bars to seat them, and do not weld within the bonded zone. Traction return cut points must be laid out sensibly at stations, or the joint can be burnt by stray current rather than worn out by traffic.
A 500 V megohmmeter is the standard tool. Read after one minute, and record both rail-to-rail and rail-to-bar resistance - they are different paths and can fail independently. One documented failure case had rail-to-rail resistance still above 10 MΩ while the rail-to-bar path had dropped to 150 Ω; when the joint was opened, the bar had debonded over roughly 100 mm from its end, forming a V-shaped pocket where dirty water collected and ate into the adhesive.

In service, an online resistance below 20 Ω calls for increased inspection frequency. Below 5 Ω the joint is normally treated as failed: clean the area, replace bolts and bushes one at a time, measure again, and if the reading does not recover, remove and re-bond. A sudden "red band" (false occupied indication) is handled the same way - first look for ballast, stray wire or water bridging the joint, then test.
Two things are worth separating. A voltage-drop alarm from the signalling side and a low insulation-resistance reading are not the same diagnosis, and a joint that passed factory acceptance can still develop a wet-path fault years later. That is why the maintenance interval matters more than the number on the original certificate.
Start with the rail section and the standard you work to: 50, 60 or 75 kg/m to TB/T 2975, 60E1 to EN 13674-1, or an AREMA section by drawing. Then give us the hole pattern and pitch, the joint length if it is a factory assembly, the bolt class, the insulation resistance required and the test method, the operating speed and axle load, and whether the joint is for a factory or field bond. A signalling drawing or the track circuit plan is worth including - it tells us where the end post has to sit relative to the sleepers.
If it is a replacement job, a photo of the failed joint and the measured rail-end gap tell us more than a paragraph of description. A drawing or an old sample is enough to confirm feasibility. We will check the profile and the drilling pattern before quoting rather than revise the price after the drawing arrives.
A bolted insulated joint isolates the rails with loose insulating parts but leaves a mechanical gap. A glued insulated joint bonds the bars to the rail web, so the assembly carries longitudinal force like continuous rail and can be welded into a CWR string while still blocking signal current.
Name the standard and the test condition. TB/T 2975-2018 asks for more than 10 MΩ dry and 1000 Ω wet for the complete joint, and more than 20 MΩ dry for the joint bar. EN 16843:2024 uses different before/after mechanical test values. Do not compare the numbers without the method.
Yes - that is the main application. Longitudinal shear capacity is 2700 kN for 50 kg/m, 3000 kN for 60 kg/m and 3300 kN for 75 kg/m rail to TB/T 2975, with a fatigue requirement of two million cycles at 180 kN. Factory hot-bonded assemblies are the usual choice for these conditions.
Yes. Every bolt passes through both joint bars, so a bare bolt or a plain steel washer gives signal current a direct metal path across the joint. Bushings and insulated washers are part of the isolation, not optional hardware.
Final tightening is at least 1100 N·m on high-strength assemblies, applied in stages and recorded. Correctly installed 12.9S bolts are specified for one-time tightening without routine re-torquing; if a joint keeps losing torque, the cause is usually a seating or bonding problem, not the bolt.
Factory hot-bonded for high-speed, heavy-haul and any job where consistency and a measured assembly length matter. Field ambient-cured for interval joints, remote sites and emergency replacement, provided the rail web can be kept dry and the temperature and humidity windows are respected.
For field bonding, ambient temperature should be above about 0 °C and relative humidity below roughly 60 %. Moisture on the bonding surface is the single most common cause of a low wet resistance reading later on.
Factory assemblies are supplied as a measured rail length with the joint already bonded; field kits are packed as a matched set of bars, end post, bushes, bolts, washers and adhesive, marked by rail section and drilling pattern. The usual document set is dimensional inspection records, bar material certificates and an insulation resistance test record; we confirm which documents apply to your order in the quotation. Third-party inspection is an option if the project calls for it, and is not included as standard.
Yes. Send the rail section, the drilling drawing and the standard you work to. We can trial-produce bonded joints to GB/T 2585, UIC 864 / EN 13674-1, AREMA or GOST rail profiles, and we confirm the specification before quoting.
Yes. Insulated fishplates, composite integral insulated joints, steel rails, crane rail fastenings, turnout components and fasteners & hardware can go into one enquiry and one shipment, which usually saves more on freight than it costs in consolidation.
Send the rail section, the standard, the hole pattern, the quantity and whether you need a factory or field bond. We can develop and trial-produce glued insulated rail joints to your drawing - GB/T 2585, UIC, AREMA or GOST sections - and will confirm the specification before quoting. A datasheet, samples or a project price are available - contact us. For a mixed order, ask about our crane rail fastenings, steel rails, insulated fishplates, railway turnout components, track maintenance tools & equipment and fasteners & hardware in the same enquiry.