A compromise fishplate joins two different rail sections - one profile at each end
Compromise, combination and transition joint bar are three names for the same made-to-order family
The running surfaces have to finish level or the wheel meets a step at the joint
Gauge-side and outside bars are handed - a full set for different head widths is four bars, not two
Hole pitch and vertical position follow each rail end, not one standard drilling chart
Forged or machined to order; grade and heat treatment follow the contract, not the rail weight
Both rail profile drawings and the height difference are required before a bar can be quoted
Where the change is permanent and welding is available, a transition rail may be the better answer
A compromise fishplate — also sold as a compromise joint bar, a combination fishplate or a rail transition joint bar — joins two rails that are not the same section. One end of the bar is shaped to the profile of the first rail and the other end to the profile of the second. A plain bar has one profile along its whole length and can only do that job when both rails match; a compromise bar is asymmetric because the two rails are.
The part has two jobs at the same time. It has to hold the two rail ends in line mechanically, and it has to carry the wheel across a change of head width, rail height and web position without a step at the running surface. The second job is what makes it a compromise rather than simply a longer bar. If the tops of the two rails finish at different heights, the wheel hits an edge, and an edge at a joint is where impact starts.
All three names are in common use. "Compromise" is the older railway term and the one most drawings use. "Combination fishplate" appears in some suppliers' catalogues for the same product. "Transition joint bar" describes what it does rather than what it is. The three labels point to the same family of made-to-order bars, and none of them is a stock item with a universal part number.
Everything below is about one joint — deciding whether a compromise bar suits the change, then fixing both profiles on a drawing before anything is ordered. What goes wrong when either step is skipped runs through the later sections. Standards and naming across the whole fishplate range are a separate subject, covered under fishplates and joint bars across all standards; here the subject is the joint at which two sections meet.
Track rarely stays one section for its whole life. A line is renewed in stages, a lighter rail meets a heavier one at the boundary between two work packages, and both ends have to run before the rest of the renewal catches up. A new industrial spur is often laid to a heavier section than the old line it ties into. At a national border or a change of standard, one rail family ends and another begins. Bridges, tunnels and turnouts can call for a different section over a short length, then return to the main-line profile.
In each case the connection is temporary in intent but permanent in service. A compromise joint may be installed as a phase of a renewal and then stay in the track for years. It inherits the whole duty: axle load, braking and traction force, temperature movement and the fatigue cycle of every wheel that crosses it.
There is an alternative worth naming. A transition rail — a short length forged or machined to taper from one profile to the other, then welded in — avoids a bolted joint at the change point. It is the preferred answer where the connection is permanent and welding is available. The bolted compromise bar remains the usual choice for phased work, temporary closures and locations where a welded special cannot be produced or installed within the possession.
The choice is an engineering decision, not a catalogue one. An enquiry can name a different rail section connection and still not need a compromise bar. What decides it is whether the change of section is a boundary that will move, or a permanent feature of the alignment — and what can be welded on site.
A standard bar is made for one profile. Its fishing faces, bar depth, hole height and hole pitch all follow that rail, and it can be rolled in long runs. A compromise bar is made for a pair of profiles. It cannot be rolled as one constant section, so it is forged or machined, and one end of it will not fit the rail at the other end.
Point | Standard fishplate | Compromise fishplate |
Rail sections | One section both sides | Two different sections |
Bar profile | Constant along the length | Different profile at each end |
Production | Rolled in long runs, then drilled or punched | Forged or machined to order |
Running surface | Set by one rail height | Must be aligned across two different heights |
Bolt holes | One pitch pattern | Pitch and sometimes diameter differ end to end |
Left / right hand | Not applicable | Handed; a full set uses four bars |
Procurement | Section and standard usually enough | Both rail drawings and site conditions required |

The consequence is commercial as much as technical. A standard bar can be quoted from a rail designation. A compromise bar cannot: two rails of the same nominal weight can have different heights, head widths and fishing angles, so the designation alone does not define the part. An enquiry that names only "50 kg to 60 kg" has named the weights and nothing else.
Four differences between two rails decide whether a compromise bar can be made to work and how it has to be detailed.
Rail height. The two heads have to finish at the same level. Where the sections differ in height, the lower rail is raised on shims or the bar is made with an offset so that the running surfaces line up at the joint. Getting this wrong is not a cosmetic fault. The Australian Transport Safety Bureau (ATSB) investigated a 2016 derailment near Rushall Station. Its report found that a lateral angular discontinuity at a mechanical rail joint produced a localised increase in wheel-to-rail lateral force, on a curve where lubrication was also deficient. The joint geometry was a contributing factor, and the train was inside the speed limit. A step or an angle at a joint changes the force the wheel sees.

Head width and gauge corner. The wheel runs on the head and the flange works against the gauge corner. A change in head width shifts where that contact happens. The bar has to hold both gauge lines as close to aligned as the two sections allow, or the wheel sees a kink as well as a step.
Web thickness and fishing angle. The bar seats on the sloping faces under the head and above the foot. Those faces sit at different angles on different sections. Each half of a compromise bar is shaped to its own rail; a bar that only approximates one side will bear on a line instead of a face, and the clamping load goes into a small contact patch.
Hole position. The bolt line sits near the neutral axis of the rail so that the drilling takes as little out of the bending section as possible. Because the two rails have different heights and web positions, the hole line is not at the same height on each half of a compromise bar. That is why the pitch and the vertical position have to come from the two rail drawings, not from a standard drilling chart.
A compromise joint is not one bar. It is a set, and the rail transition joint bar on each side of the track is shaped for its own position.
On a pair of rails with different head widths, the bar on the gauge side and the bar on the outside of the track are not the same shape. The bars are handed. The convention used on North American drawings is to stand on the gauge side of the heavier rail, facing the direction of the lighter rail. The joint on the left is then the left-hand joint, and the one on the right is the right-hand joint. A complete set for one joint is four bars — left outside, left gauge, right gauge and right outside — not two.

Some suppliers list a pair where the head-width difference is small enough that the same outline works on both sides. That exception is a design decision on the drawing, not a default to assume when ordering.
The combinations that come up most often are a heavier main-line section to a lighter siding or legacy section, and a section from one standard family to a section from another. Both ends of the pairing have to be stated: which rail is the heavier one, which standard each was rolled to, and how much they differ in height. A list of popular pairings in a catalogue is a guide to what has been made before. It is not a compatibility table for a new order, and the same nominal weights can hide different profiles.
Where the two rails are close in height and web position, a compromise bar is a reasonable answer. Where a light rail is being joined to a heavy main-line rail with a large difference in both, the joint becomes a permanent weak point even when it is made correctly. In that case a transition rail or a re-aligned replacement length deserves a look first.
The hole line on a compromise bar follows each rail's own drilling. Pitch, end distance, hole diameter and vertical position can all differ between the two halves of the same bar. Nothing here can be copied from a standard four-hole or six-hole chart.

Fish bolts are part of the joint and belong in the same order as the bars. Diameter, length, property class and head form are specified together with the nut and the washer stack. On bars using oval neck holes, the oval hole matches an oval neck on the bolt; that pairing stops the bolt turning while the nut is tightened, and round and oval combinations are not interchangeable. Where a joint is insulated, the bolts, sleeves and washers come from the insulated assembly drawing and are not substituted from a conducting joint; the insulated fishplate assemblies used for track circuits are built around that same rule.
Tightening follows the instruction for the bolt set supplied. Published torque figures for fish bolts vary widely with diameter, class, thread condition and surface treatment, so a bare number is a placeholder rather than a specification. If the project uses a given torque or a turn-of-nut method, its source should be stated in the method statement.
A compromise bar is made to order because no rolled section has one profile at each end. Forging is the usual route: a heated billet is formed in a die so the bar follows the fishing faces of both rails, and the change between the two profiles is blended rather than stepped. Machining from plate or from a forged blank is used where the geometry or the quantity calls for it. In either case the material, condition and test basis come from the project specification.
That split is recognised in the standards. AREMA Manual for Railway Engineering Chapter 4, Part 3, section 3.4 names quenched carbon-steel, microalloyed and forged compromise bars as separate families rather than treating every joint bar as one grade. A compromise bar ordered under that practice is a forged item to a plan, not a catalogue profile that happens to be longer.

Alloy and carbon steels are both quoted in this market, with heat treatment setting the strength and toughness the joint needs. There is no single grade that is right for every compromise joint: the selection follows the rail steel, the axle load and the standard named in the contract. What should not appear on a quotation is a grade with no standard edition, no condition and no test basis behind it.
The manufacturing route matters because a compromise bar carries load through an asymmetric section. The transition between the two ends is where stress concentrates, and the bolt holes at each end are in different positions relative to the bar's own centre. Forging gives a continuous grain flow through that transition; machining has to leave enough section around each hole to carry the bearing load. Either route is acceptable when the drawing says so and the inspection confirms it.
Installation is where a correct bar can still end up as a bad joint. The running surfaces of the two rails have to be level at the joint and the gauge lines have to line up before the bolts are torqued. Shimming to raise the lower rail is part of the joint detail, not a site adjustment made up on the day. If the two heads finish at different levels, stop and correct the support rather than tightening over the step.

1. Confirm the set. Check the marking and the handedness. Four bars make a complete joint on a pair of rails with different head widths; two bars are only enough where the drawing allows the same outline on both sides.
2. Check the rail ends. Clean the fishing faces and measure the height difference at the joint. Confirm the drilling on both rails matches the two ends of the bar.
3. Fit the bars. Offer up the gauge-side and outside bars in the handed positions shown on the drawing. The bar should seat on the fishing faces before any bolt is tightened.
4. Fit and tighten the bolt set. Assemble the specified bolts, nuts and washers, and tighten progressively to the instruction for the set supplied.
5. Measure after tightening. Check the running-surface step and the gauge alignment again under load. Record the values with the station reference.
6. Inspect in service. Compromise joints are more sensitive to impact than plain joints because of the asymmetric geometry. Bolt condition, the running-surface step and any fretting at the contact faces belong on the routine inspection list.
The sequence above stops at the joint itself. The wider trackwork sequence — setting the gap, the line and the final record — is set out in the rail joints and fishplate installation guide.
A compromise bar cannot be ordered from a product code. The drawing is the specification, and it has to describe both rails and the joint between them.
Item | What the drawing must fix |
Both rail sections | Designation, standard and profile drawing for each rail |
Height difference | Rail head levels before and after the joint, with the shim or offset detail |
Bar outline | Fishing faces for each profile, with the transition between them |
Hole geometry | Pitch, end distance, diameter and vertical position for each end |
Handedness | Left and right, gauge side and outside, with a four-bar set where required |
Running surface | Allowed step at the joint and how it is measured |
Material and condition | Grade, heat treatment and test basis |
Insulation | If the joint is insulated, the full insulated assembly |

The items most often missing are the rail profile drawings and the height difference. A nominal weight is not a profile, and two rails that weigh the same can have different heads, webs and fishing angles. Where an existing joint has to be replaced and no drawing survives, the bar can be measured from a sample and the two rail ends surveyed, but that survey has to record both profiles rather than one.
That measurement is made on the finished bar, in the workshop, before it ships — bar length, section height, hole diameter and pitch at each end. The photograph below is one of those checks. The reading belongs to the part being made; what a buyer should take from it is that every dimension is measured against the drawing at each end, not measured at one end and assumed at the other.
A fishplate made to join two rails of different sections. One end matches the first rail profile and the other end matches the second, so the joint can hold both rails in line and carry the wheel across the change of section.
Yes. Both names are used for the same family of made-to-order bars. "Transition joint bar" is a third name describing the same product.
No. A standard bar has one profile along its length. It will seat on one rail and bear on a line or a corner on the other, and the running surfaces will not line up.
Because the gauge-side and outside bars are not the same shape when the two rails have different head widths. Standing on the gauge side of the heavier rail facing the lighter rail gives the left and right convention. A full set for such a joint is four bars.
The bolt count follows the drawing and the rail drilling at each end. The two halves can have different pitch and, where the bolt sets differ, different hole diameters. There is no universal four-hole or six-hole rule for a compromise bar.
Send both rail designations with profile drawings, the height difference measured at the joint, whether the track is jointed or continuously welded, the hole and bolt requirements, and the material and inspection basis the project names. With those in hand the bar can be quoted. Without the two profiles, a nominal weight will not produce a firm price, because two rails of the same weight can differ in head, web and fishing angle.
Yes, to a drawing showing both sections. The two profiles are set out on the UIC54 and UIC60 fishplates page, but the bar itself is not a standard UIC item: it has to be detailed for both profiles and for the height difference between them, and the designation alone does not fix the geometry.
No joint is. A compromise joint carries an asymmetric geometry and needs correct alignment and bolt preload to perform. Where the connection is permanent and welding is available, a transition rail may be the better engineering answer.
Against the drawing: both end profiles, length, hole geometry at each end, handedness, material and heat-treatment records, and the finish. The running-surface alignment is checked at installation and again in service.
Yes. Bolts, nuts and washers are supplied to match the bar drawing, including oval neck combinations where specified. Insulated joints use the insulated bolt set.
Send the two rail sections with their profile drawings and the height difference at the joint. If the sections are only known by name, state both names and the survey can be planned from there. Bars are quoted to the confirmed drawing, and inspection records go out with the goods. The wider joint bar range sits under rail joints and fishplate products; for a specific transition, use the Contact Us page.